Is a magnet a reliable grade check for stainless sections?

Magnetic response at a section corner or near a weld does not by itself prove that the wrong grade was delivered.

Magnetic response at a section corner or near a weld does not by itself prove that the wrong grade was delivered.

Technical considerations

Magnetic response at a section corner or near a weld does not by itself prove that the wrong grade was delivered. Forming and welding can alter local microstructure in an austenitic product, while ferritic grades are magnetic by nature. Lack of attraction does not confirm grade 316 either. Acceptance should use identification, batch-linked documentation and suitable analysis if required. Make the limits of quick field checks clear to purchasing staff. A critical material decision should not rely only on surface appearance or one hand-held test.

Do not confuse a field check with documentation

A section may respond more strongly at a corner than on a flat face; do not name the whole grade from one location. If doubt remains, review markings, documents and an appropriate analysis plan together. Define the sample and batch scope of that analysis. Continuing to cut and mix material before identity is resolved can make later traceability much harder.

Is corner magnetism alone grounds for rejection?

It does not establish grade by itself; apply the agreed technical acceptance requirements.

Share the material, grade, dimensions and quantity so our sales team can assess your request.