Tube bending depends on centreline radius, outside diameter and wall thickness together.
Technical considerations
Tube bending depends on centreline radius, outside diameter and wall thickness together. A tight radius may increase inner-wall wrinkling and outer-wall thinning, while the section can become oval. Mandrel support and tooling condition matter alongside grade and machine settings. State whether the drawing's radius refers to the inside surface or the tube centreline. Inspect angle, ovality and end position on the first piece. If another component must pass through the bend, verify the actual minimum clearance after forming rather than relying on the original nominal bore.
Approve the first bend by measurement
For the first trial, record minimum bore, section diameters in two directions and end positions rather than checking angle alone. Review repeatability with the same tooling, material and setup. Visible parts also need examination for tool marks. If allowable ovality or thinning has not been defined, obtain acceptance limits from the designer before committing to production.
Where is bend radius measured?
The drawing must state it explicitly; centreline radius and inside radius are different dimensions.